Time:2024.12.25Browse:0
1. Large internal polarization;
2. The electrode absorbs water and reacts with the electrolyte, causing a gas bubble;
3. The quality and performance issues of the electrolyte itself;
4. The amount of liquid injected cannot meet the process requirements;
5. Poor sealing performance of laser welding during the assembly process, resulting in air leakage during leak detection;
6. Dust and polar dust can first cause micro short circuits;
7. The positive and negative electrode plates are thicker than the process range, making it difficult to insert into the shell;
8. Liquid injection sealing problem, poor sealing performance of steel balls leading to air bubbles;
9. The incoming material of the shell has a thick shell wall, and the deformation of the shell affects the thickness;
10. The high temperature outside is also the main cause of the explosion.